Scrap rarely comes from one dramatic mistake. It accumulates from five settings that drift apart over a shift. Getting them stable is usually worth more than any single equipment upgrade.

1. Alloy temperature

Pour too cold and the metal freezes before it fills the cavity, giving laps, cold shuts and short fills. Pour too hot and you burn the release agent, oxidise the melt and shorten die life. The right window is narrow and it moves with alloy grade and shot weight. Measure at the pot, not at the nozzle, and log it per shift.

2. Die or mould temperature

A die that is too cold chills the surface and produces flow marks; too hot and the part sticks, warps or sinks. Thermal balance matters more than any single reading — the difference between the fixed and moving half often explains one-sided defects. Warm-up procedure is part of the setting, not a preliminary step.

3. Cycle time

Cycle time controls how much heat leaves the tool per part. Shortening it to chase output raises die temperature and can push you into soldering and shrinkage porosity. The stable cycle is the one that holds the same die-face temperature at the end of the shift as at the start.

4. Venting

Trapped air shows up as rounded edges, dark burn marks and internal porosity that only appears after machining. Vent area, vent depth and the position of the overflow matter more than total vent count. If you machine the part after casting and suddenly see porosity, suspect venting before you suspect the alloy.

5. Ejection and draft

Insufficient draft, or ejection that starts before the part has enough strength, produces drag marks and cracked corners. These are often accepted as cosmetic until they become the start of a fatigue failure in service. Check draft on the drawing stage, not after the tool is cut.

Making the five settings stick